Press the 'Start' button.
Then move the slider to observe the amount of curvature in the bonded
strips at different temperatures.
Fe
Al
PC
E / GPa
210
70
2
α
(microstrain K−1)
15
24
90
Poisson ratio, ν
0.26
0.33
0.35
strip thickness = 1 mm
Κ / m−1
Temperature / °C
Select your parameters and press the 'Start' button.
Then change the temperature slider and see how the
curvature changes.
Press 'Reset' to change parameters (material and
thickness, and note any changes to curvature.
Material A
Material B
E / GPa
α
(microstrain K−1)
Poisson ratio, ν