Browse the Library
Categories > Metal or alloy > Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) > Keyword: iron
2 micrographs available, ordered by micrograph number.
Micrograph
370
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
371
:
As cast white cast iron System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%) Reflected light microscopy 100 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.