Micrograph
378
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 400 μm |
|
Micrograph
379
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 200 μm |
|
Micrograph
380
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 100 μm |