Categories > Metal or alloy > Cu 70, Zn 30 (wt%) (pure) > Reflected light microscopy > Keyword: dendrite

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 425 Micrograph 425 : Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure)
Reflected light microscopy
800 μm
Link to full record for micrograph 426 Micrograph 426 : Cu 70, Zn 30 (wt%) (pure) brass, dendritic solidification
System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) (pure)
Reflected light microscopy
400 μm