Categories > Metal or alloy > Cu 60, Zn 40 (wt%) > Reflected light microscopy > Keyword: copper

5 micrographs available, ordered by micrograph number.


Link to full record for micrograph 36 Micrograph 36 : Cu 60, Zn 40 (wt%), quenched - metastable b grains
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 49 Micrograph 49 : Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 50 Micrograph 50 : Cu 60, Zn 40 (wt%), slow cooling - equiaxed grains
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 51 Micrograph 51 : Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 52 Micrograph 52 : Cu 60, Zn 40 (wt%), air cooled - Widmanstätten microstructure
System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%)
Reflected light microscopy
80 μm