2 micrographs available, ordered by micrograph number.
Micrograph
41
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 400 μm |
|
Micrograph
42
:
Zn, cold rolled - mechanical twins System: Zn, Composition: Not specified Reflected light microscopy 80 μm |