Browse the Library
Categories > Metal or alloy > Fe-C-X > Fe, C 0.2 (wt%) > Reflected light microscopy > Keyword: mechanical twins
2 micrographs available, ordered by micrograph number.
Micrograph
43
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
44
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 80 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.