Categories > Metal or alloy > Fe, C 0.2 (wt%) > Reflected light microscopy > Keyword: alloy

8 micrographs available, ordered by micrograph number.


Link to full record for micrograph 43 Micrograph 43 : Fe, C 0.2 (wt%), explosively deformed - mechanical twins
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 44 Micrograph 44 : Fe, C 0.2 (wt%), explosively deformed - mechanical twins
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
80 μm
Link to full record for micrograph 207 Micrograph 207 : Normalised low carbon manganese steel, taken transverse to directionality
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 208 Micrograph 208 : Normalised low carbon manganese steel, taken transverse to directionality
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 209 Micrograph 209 : As cast carbon steel
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 210 Micrograph 210 : As cast carbon steel
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 211 Micrograph 211 : Normalised carbon steel
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 212 Micrograph 212 : Normalised carbon steel
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
200 μm