Categories > Metal or alloy > Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al > Reflected light microscopy, cross-polarised, with Nomarski filter

6 keywords available. The number of micrographs available is given in [brackets].


alloy [8] Link to MATTER Glossary entry
Show relevant: micrographs

metal [8]
Show relevant: micrographs

nickel [8]
Show relevant: micrographs

nickel-based superalloy [8]
Show relevant: micrographs

niobium [8]
Show relevant: micrographs

precipitation [8] Link to MATTER Glossary entry
Show relevant: micrographs