Categories > Metal or alloy > Fe, C 0.12, Mn 14.2, Cr 13.7 > Scanning electron microscopy (SEM) > Keyword: stainless steel
1 micrograph available, ordered by micrograph number.
Micrograph
831
:
Austenitic stainless steel water quenched, with a-martensite needles within lamellae System: Fe-C-X, Composition: Fe, C 0.12, Mn 14.2, Cr 13.7 Scanning electron microscopy (SEM) 4 μm |