Categories > Metal or alloy > Stainless steel with Cr 15, Ni 35, Ti 5, C 0.1 > Scanning electron microscopy (SEM)
1 micrograph available, ordered by micrograph number.
Micrograph
817
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Ti 5, C 0.1 Scanning electron microscopy (SEM) 2 μm |