Categories > Metal or alloy > Fe, C 1.15, Mn 13 (wt%) > Scanning electron microscopy (SEM) > Keyword: austenite
1 micrograph available, ordered by micrograph number.
Micrograph
821
:
Austenitic stainless steel impact deformed at room temperature System: Fe-C-X, Composition: Fe, C 1.15, Mn 13 (wt%) Scanning electron microscopy (SEM) 2.5 μm |