Browse the Library
Categories > Metal or alloy > Not specified (Pb) > Transmitted light microscopy
4 micrographs available, ordered by micrograph number.
Micrograph
894
:
Hunan province China. Lead-zink-slag System: Pb, Composition: Not specified Transmitted light microscopy 100 μm |
|
Micrograph
895
:
Hunan province China. Lead-zink-slag System: Pb, Composition: Not specified Transmitted light microscopy 100 μm |
|
Micrograph
971
:
Sierra de Gador, Almeria, Spain. Subrecent lead slag System: Pb, Composition: Not specified Transmitted light microscopy 1 mm |
|
Micrograph
973
:
Dasht-e-Kavir, Saghand, Central Iran. Lead slag System: Pb, Composition: Not specified Transmitted light microscopy 500 μm |