Categories > Metal or alloy > Al 64, Cu 36 (wt%) > Reflected light microscopy > Keyword: aluminium

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 5 Micrograph 5 : Al 64, Cu 36 (wt%), hypereutectic alloy
System: Al-Cu, Composition: Al 64, Cu 36 (wt%)
Reflected light microscopy
400 μm