Link to full record for micrograph 82 Micrograph 82 : Aluminium, fracture surface
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
15 μm
Link to full record for micrograph 83 Micrograph 83 : Aluminium, fracture surface
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 635 Micrograph 635 : Open celled aluminium foam produced by infiltration of sintered salt
System: Al, Composition: Not specified
Scanning electron microscopy (SEM)
400 μm