Categories > Metal or alloy > Wrought iron (plain carbon steel) > Keyword: directionality
2 micrographs available, ordered by micrograph number.
Micrograph
201
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 400 μm |
|
Micrograph
202
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 200 μm |