Browse the Library
Categories > Metal or alloy > Keyword: lamella
15 micrographs available, ordered by micrograph number.
Showing 11 - 15 of 15 micrographs | Page 1 2 | Previous | Next |
Micrograph
666
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
667
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
668
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 50 μm |
|
Micrograph
669
:
Al-90 wt% Cu (bronze) System: Al-Cu, Composition: Al 10, Cu 90 (wt%) Reflected light microscopy 20 μm |
|
Micrograph
778
:
Grey cast iron (flake graphite) System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%) Reflected light microscopy 40 μm |
Showing 11 - 15 of 15 micrographs | Page 1 2 | Previous | Next |