Link to full record for micrograph 137 Micrograph 137 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 138 Micrograph 138 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 139 Micrograph 139 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 140 Micrograph 140 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 141 Micrograph 141 : Al-Mg-Si, failed through microvoid coalescence.
System: Al-Mg-Si, Composition: Al, Si 1.2, Mg 0.4 (wt%) (AA6016)
Scanning electron microscopy (SEM)
40 μm
Link to full record for micrograph 142 Micrograph 142 : Tough pitch copper, failed by fibrous ductile fracture.
System: Cu, Composition: Tough pitch copper
Scanning electron microscopy (SEM)
20 μm
Link to full record for micrograph 780 Micrograph 780 : Heat treated spheroidal graphite cast iron
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 781 Micrograph 781 : Heat treated spheroidal graphite cast iron
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 782 Micrograph 782 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 783 Micrograph 783 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm

Showing 1 - 10 of 23 micrographs Page 1 2 3 | Previous | Next

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.