Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Metal or alloy > Keyword: heat treatment

9 micrographs available, ordered by micrograph number.


Link to full record for micrograph 657 Micrograph 657 : Al-4 wt% Cu, age hardened alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 658 Micrograph 658 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 659 Micrograph 659 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 660 Micrograph 660 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 661 Micrograph 661 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 662 Micrograph 662 : Al-4 wt% Cu, over aged alloy
System: Al-Cu, Composition: Al 96, Cu 4 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 726 Micrograph 726 : Ni-Superalloy, heat treated above gamma-prime solvus
System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy)
Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode
10 μm
Link to full record for micrograph 780 Micrograph 780 : Heat treated spheroidal graphite cast iron
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 781 Micrograph 781 : Heat treated spheroidal graphite cast iron
System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%)
Reflected light microscopy
50 μm

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.