Categories > Metal or alloy > Keyword: brittle

6 micrographs available, ordered by micrograph number.


Link to full record for micrograph 78 Micrograph 78 : Forging steel, brittle, intergranular fracture
System: Fe-C-X, Composition: Forging steel
Scanning electron microscopy (SEM)
800 μm
Link to full record for micrograph 143 Micrograph 143 : Notched low carbon ferritic steel, failed through cleavage.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
20 μm
Link to full record for micrograph 144 Micrograph 144 : Zinc, notched specimen, failed through brittle cleavage fracture.
System: Zn, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 145 Micrograph 145 : Zinc, notched specimen, failed through brittle cleavage fracture.
System: Zn, Composition: Not specified
Scanning electron microscopy (SEM)
1 mm
Link to full record for micrograph 146 Micrograph 146 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 147 Micrograph 147 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm