2 micrographs available, ordered by micrograph number.
Micrograph
615
:
Cross-section of an aluminium casting System: Al, Composition: Commercial purity (99.5%) Reflected light microscopy 10 mm |
|
Micrograph
656
:
Al, commercial purity System: Al, Composition: Not specified Reflected light microscopy 10 mm |