Browse the Library
Categories > Metal or alloy > Cu-Zn > Cu 70, Zn 30 (wt%) > Reflected light microscopy > Keyword: zinc
8 micrographs available, ordered by micrograph number.
Micrograph
29
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
30
:
Cu 70, Zn 30 (wt%), annealed and cold rolled System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
31
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
32
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
33
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
34
:
Cu 70, Zn 30 (wt%), partial recrystallisation - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
35
:
Cu 70, Zn 30 (wt%), faster recrystallisation - finer grain size System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
37
:
Cu 70, Zn 30 (wt%), slow cooling - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |