Browse the Library
Categories > Metal or alloy > Cu-Zn > Cu 60, Zn 40 (wt%) + Pb trace > Reflected light microscopy > Keyword: zinc
4 micrographs available, ordered by micrograph number.
Micrograph
443
:
Commercial grade free machining brass - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 400 μm |
|
Micrograph
444
:
Commercial grade free machining brass - Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 200 μm |
|
Micrograph
445
:
Cast and annealed 40 wt% Zn brass System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 400 μm |
|
Micrograph
446
:
Cast and annealed 40 wt% Zn brass System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) + Pb trace Reflected light microscopy 200 μm |
Help is available on browsing.