Categories > Metal or alloy > Cu-Zn > Cu 55, Zn 45 (wt%) > Reflected light microscopy > Keyword: zinc
6 micrographs available, ordered by micrograph number.
Micrograph
449
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
450
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
451
:
Cu 55, Zn 45 (wt%) brass, rapidly cooled System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
455
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
456
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
457
:
Cu 55, Zn 45 (wt%) brass, as cast, dendritic System: Cu-Zn, Composition: Cu 55, Zn 45 (wt%) Reflected light microscopy 200 μm |