Browse the Library
Categories > Metal or alloy > Cu-Zn > Cu 52.5, Zn 47.5 (wt%) > Reflected light microscopy > Keyword: alloy
3 micrographs available, ordered by micrograph number.
Micrograph
452
:
Cu 52.5, Zn 47.5 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
453
:
Cu 52.5, Zn 47.5 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
454
:
Cu 52.5, Zn 47.5 (wt%) brass, as cast System: Cu-Zn, Composition: Cu 52.5, Zn 47.5 (wt%) Reflected light microscopy 200 μm |
Help is available on browsing.