Browse the Library
Categories > Metal or alloy > Cu-Zn > Cu 50, Zn 50 (wt%) > Reflected light microscopy > Keyword: alloy
3 micrographs available, ordered by micrograph number.
Micrograph
472
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
473
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
474
:
Cu 50, Zn 50 (wt%) brass, chill cast System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%) Reflected light microscopy 100 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.