Browse the Library
Categories > Metal or alloy > Cu-Zn > Keyword: annealing
18 micrographs available, ordered by micrograph number.
Showing 11 - 18 of 18 micrographs | Page 1 2 | Previous | Next |
Micrograph
429
:
Cu 70, Zn 30 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
430
:
Cu 70, Zn 30 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 70, Zn 30 (wt%) Reflected light microscopy 100 μm |
|
Micrograph
431
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
432
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
433
:
Cu 90, Zn 10 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 90, Zn 10 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
434
:
Cu 90, Zn 10 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 90, Zn 10 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
475
:
Cu 55, Zn 45 (wt%) brass, cast annealed System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
476
:
Cu 55, Zn 45 (wt%) brass, cast annealed System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%) Reflected light microscopy 400 μm |
Showing 11 - 18 of 18 micrographs | Page 1 2 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.