Showing 51 - 60 of 64 micrographs Page 1 2 3 4 5 6 7 | Previous | Next

Link to full record for micrograph 460 Micrograph 460 : Brass, exhibiting grain boundary nucleation
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 468 Micrograph 468 : Cu 50, Zn 50 (wt%) brass, as cast
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 469 Micrograph 469 : Cu 50, Zn 50 (wt%) brass, as cast
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 470 Micrograph 470 : Cu 50, Zn 50 (wt%) brass, as cast
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 471 Micrograph 471 : Cu 50, Zn 50 (wt%) brass, as cast
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 472 Micrograph 472 : Cu 50, Zn 50 (wt%) brass, chill cast
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 473 Micrograph 473 : Cu 50, Zn 50 (wt%) brass, chill cast
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 474 Micrograph 474 : Cu 50, Zn 50 (wt%) brass, chill cast
System: Cu-Zn, Composition: Cu 50, Zn 50 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 475 Micrograph 475 : Cu 55, Zn 45 (wt%) brass, cast annealed
System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 476 Micrograph 476 : Cu 55, Zn 45 (wt%) brass, cast annealed
System: Cu-Zn, Composition: Cu 52, Zn 45 (wt%)
Reflected light microscopy
400 μm