Categories > Metal or alloy > Fe-C-X > Fe, C 1.0 (wt%) > Keyword: iron

6 micrographs available, ordered by micrograph number.


Link to full record for micrograph 21 Micrograph 21 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 22 Micrograph 22 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 23 Micrograph 23 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
50 μm
Link to full record for micrograph 24 Micrograph 24 : Fe, C 1.0 (wt%), hypereutectoid alloy
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Scanning electron microscopy (SEM)
10 μm
Link to full record for micrograph 253 Micrograph 253 : Fe, C 1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 254 Micrograph 254 : Fe, C 1 (wt%) steel, normalised hypereutectoid
System: Fe-C-X, Composition: Fe, C 1.0 (wt%)
Reflected light microscopy
200 μm