Categories > Metal or alloy > Fe-C-X > Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) > Keyword: steel

7 micrographs available, ordered by micrograph number.


Link to full record for micrograph 328 Micrograph 328 : Nickel low carbon steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 329 Micrograph 329 : Nickel low carbon steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 340 Micrograph 340 : Low alloy medium carbon steel, containing Ni, Cr, Mo, annealed
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 341 Micrograph 341 : Low alloy medium carbon steel, containing Ni, Cr, Mo, annealed
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 342 Micrograph 342 : Medium carbon, low alloy steel
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 343 Micrograph 343 : Medium carbon, low alloy steel
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 344 Micrograph 344 : Medium carbon, low alloy steel.
System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%)
Reflected light microscopy
100 μm