Link to full record for micrograph 362 Micrograph 362 : White cast iron, subject to slow heating and cooling treatment
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 363 Micrograph 363 : White cast iron, subject to slow heating and cooling treatment
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 364 Micrograph 364 : White cast iron, subject to slow heating and cooling treatment
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%)
Reflected light microscopy
100 μm