Link to full record for micrograph 356 Micrograph 356 : Pearlitic malleable cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 357 Micrograph 357 : Pearlitic malleable cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 358 Micrograph 358 : White cast iron, annealed to precipitate out carbon
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 359 Micrograph 359 : White cast iron, annealed to precipitate out carbon
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 360 Micrograph 360 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 361 Micrograph 361 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 368 Micrograph 368 : Blackheart cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 369 Micrograph 369 : Blackheart cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
200 μm

Help is available on browsing.

Alternatively, search the Library (from top right on any page), or use advanced search.