Categories > Metal or alloy > Fe-C-X > Fe, C 0.9 (wt%) > Atomic force microscopy (AFM)

5 micrographs available, ordered by micrograph number.


Link to full record for micrograph 864 Micrograph 864 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
2 μm
Link to full record for micrograph 865 Micrograph 865 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
10 μm
Link to full record for micrograph 866 Micrograph 866 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
5 μm
Link to full record for micrograph 867 Micrograph 867 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
2 μm
Link to full record for micrograph 871 Micrograph 871 : Low Carbon Steel
System: Fe-C-X, Composition: Fe, C 0.9 (wt%)
Atomic force microscopy (AFM)
30 μm