Categories > Metal or alloy > Fe-C-X > Grey cast iron > Keyword: metal

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 381 Micrograph 381 : Grey cast iron
System: Fe-C-X, Composition: Grey cast iron
Reflected light microscopy
400 μm
Link to full record for micrograph 382 Micrograph 382 : Grey cast iron
System: Fe-C-X, Composition: Grey cast iron
Reflected light microscopy
200 μm
Link to full record for micrograph 383 Micrograph 383 : Grey cast iron
System: Fe-C-X, Composition: Grey cast iron
Reflected light microscopy
100 μm