Categories > Metal or alloy > Fe-C-X > Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) > Keyword: ductile

13 micrographs available, ordered by micrograph number.


Showing 1 - 10 of 13 micrographs Page 1 2 | Previous | Next

Link to full record for micrograph 782 Micrograph 782 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 783 Micrograph 783 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 784 Micrograph 784 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 785 Micrograph 785 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 786 Micrograph 786 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 787 Micrograph 787 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 788 Micrograph 788 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 789 Micrograph 789 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
40 μm
Link to full record for micrograph 790 Micrograph 790 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 791 Micrograph 791 : Austempered ductile cast iron
System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%)
Reflected light microscopy
100 μm