Link to full record for micrograph 799 Micrograph 799 : Austenitic stainless steel solution treated, water quenched and tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Scanning electron microscopy (SEM)
2 μm
Link to full record for micrograph 801 Micrograph 801 : Austenitic stainless steel solution treated, water quenched then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
400 nm
Link to full record for micrograph 802 Micrograph 802 : Austenitic stainless steel solution treated, water quenched then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 803 Micrograph 803 : Austenitic stainless steel solution treated, water quenched then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 809 Micrograph 809 : Austenitic stainless steel solution treated, quenched, deformed in tension, then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 814 Micrograph 814 : Austenitic stainless steel solution treated, quenched and tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 822 Micrograph 822 : Austenitic stainless steel tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Transmission electron microscopy (TEM)
400 nm
Link to full record for micrograph 833 Micrograph 833 : Austenitic stainless steel solution treated, quenched then tempered
System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%)
Reflected light microscopy