Categories > Metal or alloy > Fe-C-X > Fe, C 0.2, Mo 4 (wt%) > Keyword: ferrite

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 823 Micrograph 823 : Martensitic steel tempered, with dislocation helices in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 824 Micrograph 824 : Martensitic steel tempered, with precipitation of Mo2C in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
1 μm
Link to full record for micrograph 828 Micrograph 828 : Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm
Link to full record for micrograph 829 Micrograph 829 : Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite
System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%)
Transmission electron microscopy (TEM)
500 nm