Categories > Metal or alloy > Fe-C-X > Fe, Mn 1, S 0.02 (wt%) > Scanning electron microscopy (SEM)

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 810 Micrograph 810 : Ferritic steel heat treated and water quenched
System: Fe-C-X, Composition: Fe, Mn 1, S 0.02 (wt%)
Scanning electron microscopy (SEM)
1.5 μm