Categories > Metal or alloy > Fe-C-X > Fe, C 0.20, Mo 3.8, Ta 0.22 (wt%) > Keyword: austenite

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 826 Micrograph 826 : Austenitic stainless steel tempered, with Mo2 and M6C precipitates
System: Fe-C-X, Composition: Fe, C 0.20, Mo 3.8, Ta 0.22 (wt%)
Scanning electron microscopy (SEM)
2.5 μm