Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

DoITPoMS Micrograph Library Browse the Library

Browse the Library

Categories > Metal or alloy > Fe-C-X > Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) > Keyword: cast iron

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 72 Micrograph 72 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 73 Micrograph 73 : Ni-hard iron
System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron)
Reflected light microscopy
80 μm