Categories > Metal or alloy > Fe-C-X > Fe, C 0.24, Si 2.18, Mn 2.32, Ni 1.05 (wt%) > Keyword: shape deformation

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 133 Micrograph 133 : Steel, austenitised at 1200 centigrade for 120 s and then transformed isothermally at 350 centigrade for 2000 s before cooling to room temperature.
System: Fe-C-X, Composition: Fe, C 0.24, Si 2.18, Mn 2.32, Ni 1.05 (wt%)
Atomic force microscopy (AFM)
1 μm