Categories > Metal or alloy > Fe-C-X > Not specified > Keyword: brittle

3 micrographs available, ordered by micrograph number.


Link to full record for micrograph 143 Micrograph 143 : Notched low carbon ferritic steel, failed through cleavage.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
20 μm
Link to full record for micrograph 146 Micrograph 146 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm
Link to full record for micrograph 147 Micrograph 147 : HY100 forging steel, notched impact specimen, failed through brittle intergranular fracture.
System: Fe-C-X, Composition: Not specified
Scanning electron microscopy (SEM)
200 μm