Categories > Metal or alloy > Fe-C-X > Fe, C 0.07, Mn 2.2 (wt%) > Keyword: metal
7 micrographs available, ordered by micrograph number.
Micrograph
271
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 800 μm |
|
Micrograph
272
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
273
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
274
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
275
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
276
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
277
:
Fe, C 0.07, Mn 2.3 (wt%) steel, carburised at 950°C System: Fe-C-X, Composition: Fe, C 0.07, Mn 2.2 (wt%) Reflected light microscopy 200 μm |