Categories > Metal or alloy > Fe-C-X > Fe, C 0.2 (wt%) > Keyword: steel

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 281 Micrograph 281 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 282 Micrograph 282 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 283 Micrograph 283 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 284 Micrograph 284 : Fe, C 0.2 (wt%) steel, case hardened
System: Fe-C-X, Composition: Fe, C 0.2 (wt%)
Reflected light microscopy
100 μm