Link to full record for micrograph 294 Micrograph 294 : Fe, C 0.75 (wt%) steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.75 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 295 Micrograph 295 : Fe, C 0.75 (wt%) steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.75 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 296 Micrograph 296 : Fe, C 0.75 (wt%) steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.75 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 297 Micrograph 297 : Fe, C 0.75 (wt%) steel, quenched, martensitic and quench cracks
System: Fe-C-X, Composition: Fe, C 0.75 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 298 Micrograph 298 : Fe, C 0.75 (wt%) steel, quenched, martensitic and quench cracks
System: Fe-C-X, Composition: Fe, C 0.75 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 299 Micrograph 299 : Fe, C 0.75 (wt%) steel, quenched, martensitic and manganese sulphides
System: Fe-C-X, Composition: Fe, C 0.75 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 300 Micrograph 300 : Fe, C 0.75 (wt%) steel, quenched, martensitic and manganese sulphides
System: Fe-C-X, Composition: Fe, C 0.75 (wt%)
Reflected light microscopy
100 μm