Categories > Metal or alloy > Fe-C-X > Fe, C 0.3 (wt%) > Keyword: carbon

7 micrographs available, ordered by micrograph number.


Link to full record for micrograph 303 Micrograph 303 : Fe, C 0.3 (wt%) steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 304 Micrograph 304 : Fe, C 0.3 (wt%) steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 305 Micrograph 305 : Fe, C 0.3 (wt%) steel, quenched and tempered
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 333 Micrograph 333 : Medium carbon steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 334 Micrograph 334 : Medium carbon steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 335 Micrograph 335 : Medium carbon steel, slow quenched
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 336 Micrograph 336 : Medium carbon steel, quenched
System: Fe-C-X, Composition: Fe, C 0.3 (wt%)
Reflected light microscopy
200 μm