Categories > Metal or alloy > Fe-C-X > Keyword: cementite
14 micrographs available, ordered by micrograph number.
Showing 11 - 14 of 14 micrographs | Page 1 2 | Previous | Next |
Micrograph
26
:
Fe, C 0.85 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 0.85 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
66
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
|
Micrograph
67
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 80 μm |
|
Micrograph
778
:
Grey cast iron (flake graphite) System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5 (wt%) Reflected light microscopy 40 μm |