Categories > Metal or alloy > Fe-C-X > Keyword: ferrite
35 micrographs available, ordered by micrograph number.
Showing 31 - 35 of 35 micrographs | Page 1 2 3 4 | Previous | Next |
Micrograph
810
:
Ferritic steel heat treated and water quenched System: Fe-C-X, Composition: Fe, Mn 1, S 0.02 (wt%) Scanning electron microscopy (SEM) 1.5 μm |
|
Micrograph
823
:
Martensitic steel tempered, with dislocation helices in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
824
:
Martensitic steel tempered, with precipitation of Mo2C in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 1 μm |
|
Micrograph
828
:
Martensitic steel tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |
|
Micrograph
829
:
Martensitic steel quenched then tempered, with precipitation of Mo2C on dislocations in ferrite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Transmission electron microscopy (TEM) 500 nm |