Categories > Metal or alloy > Fe-C-X > Keyword: metal
281 micrographs available, ordered by micrograph number.
Showing 11 - 20 of 281 micrographs | Page 1 2 3 4 5 6 7 .. 29 | Previous | Next |
Micrograph
24
:
Fe, C 1.0 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 1.0 (wt%) Scanning electron microscopy (SEM) 10 μm |
|
Micrograph
25
:
Fe, C 0.85 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 0.85 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
26
:
Fe, C 0.85 (wt%), hypereutectoid alloy System: Fe-C-X, Composition: Fe, C 0.85 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
27
:
Fe, C 0.9 (wt%), martensite System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Reflected light microscopy 40 μm |
|
Micrograph
28
:
Fe, C 0.9 (wt%), martensite System: Fe-C-X, Composition: Fe, C 0.9 (wt%) Scanning electron microscopy (SEM) 10 μm |
|
Micrograph
43
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
44
:
Fe, C 0.2 (wt%), explosively deformed - mechanical twins System: Fe-C-X, Composition: Fe, C 0.2 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
45
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
46
:
Fe, Ni 30, C 0.3 (wt%), quenched - martensite plates System: Fe-C-X, Composition: Fe, C 0.3, Ni 30 (wt%) Reflected light microscopy 80 μm |
|
Micrograph
62
:
Fe, C 3.6, Si 2.1 (wt%), hypereutectic grey cast iron System: Fe-C-X, Composition: Fe, C 3.6, Si 2.1 (wt%) Reflected light microscopy 400 μm |