73
:
Ni-hard iron System: Fe-C-X, Composition: Fe, C 2.8, Ni 4.5, Mn 1.2, Cr 0.75, Si 0.5, P 0.3, Mo 0.25, S 0.1 (wt% typical) (Ni-hard iron) Reflected light microscopy 80 μm |
|
Micrograph
78
:
Forging steel, brittle, intergranular fracture System: Fe-C-X, Composition: Forging steel Scanning electron microscopy (SEM) 800 μm |
|
Micrograph
134
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 600 nm |
|
Micrograph
135
:
High carbon steel System: Fe-C-X, Composition: Fe, C 1, Mn 2, Si 1.5, Cr 1.3 (wt%) Transmission electron microscopy (TEM) 1.5 μm |
|
Micrograph
201
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 400 μm |
|
Micrograph
202
:
Normalised low carbon steel, showing directionality System: Fe-C-X, Composition: Wrought iron (plain carbon steel) Reflected light microscopy 200 μm |
|
Micrograph
203
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
204
:
Normalised low carbon manganese steel, showing directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |
|
Micrograph
205
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 400 μm |
|
Micrograph
206
:
Normalised low carbon manganese steel, taken transverse to directionality System: Fe-C-X, Composition: Fe, C 0.1, Mn 1, S 0.5 (wt%) Reflected light microscopy 200 μm |